Reference illustration — produced to your drawing
Nuts
Weld Nut Retainers
A weld nut retainer holds a nut in a fixed position on a panel so it can be welded or bolted in place during assembly. The retainer keeps the nut aligned while the mating bolt is driven.
Used in sheet-metal assemblies where a nut must be fixed and aligned for blind bolting, such as appliance panels and enclosures. Bought by sheet-metal fabricators.
Standard
To your drawing
Size range
M4 – M12
MOQ
From 50 pcs
Lead time
Samples 5–10 days
What we produce
- Carbon steel 1045 or stainless steel 304
- Formed retainer or cage holds the nut in place
- Metric coarse or UNC internal thread
- Zinc-plated or plain finish
- Made by stamping and welding
Specification notes
- Retainer geometry is set per drawing
- Minimum order quantity starts from 50 pieces
Specifications
Every line below is a starting point, not a limit. Non-standard sizes, special threads and unusual materials are what we do — send the drawing and we confirm what fits.
| Size range | M4 – M12 |
|---|---|
| Threads | Metric coarse · UNC |
| Head / geometry | Weld nut held in a formed retainer or cage; no drive recess |
| Materials | Stainless steel 301 / 303 / 304 / 304L / 316 / 316L / 410 / 416 / 17-4PH · carbon steel 1045 / 1215 / 12L14 · alloy steel 4130 / 4140 · aluminium 2024 / 5052 / 6061 / 7075 · brass · bronze · copper · titanium |
| Finishes | As machined · black oxide · zinc plating · nickel plating · chrome plating · anodizing · passivation (through our vetted partner network) |
| Precision | ±0.01 mm on features that locate, seal or fit; ISO 2768-m for general dimensions |
| Marking | Head marking, grade marking or your own identification mark per drawing |
| Documents | Material certificate (MTR) with every batch, plus pre-shipment photos before dispatch |
| MOQ | From 50 pieces per type and material · samples from 1 piece |
| Sample lead time | 5–10 days |
| Production lead time | 25–35 days after sample approval |
| Quote | Within 24 hours, with DFM feedback |
Other nuts we manufacture
See all 179 part types →Send us the drawing