Reference illustration — produced to your drawing
Nails & Spikes
Pallet Nails
Pallet nails have a ring or screw shank that holds pallet boards and blocks together under load and handling. The deformed shank grips wood fibre to resist loosening.
Used in pallet and crate manufacturing and repair. Bought by pallet makers and industrial packaging plants.
Standard
ASTM F1667
Size range
1 1/2 – 3 1/2 in · 38 – 89 mm
MOQ
From 50 pcs
Lead time
Samples 5–10 days
What we produce
- Ring or screw shank for high withdrawal resistance
- Flat head seats flush with the deck board
- Cold headed from drawn carbon steel wire
- Diamond point drives quickly through deck boards
- Bright or electro-galvanized finish
Specification notes
- Common lengths from 2 in to 3 1/2 in (51 – 89 mm)
- Custom lengths and shank styles per drawing
- Material certificate and pre-shipment photos provided
Specifications
Every line below is a starting point, not a limit. Non-standard sizes, special threads and unusual materials are what we do — send the drawing and we confirm what fits.
| Standard | ASTM F1667 |
|---|---|
| Size range | 1 1/2 – 3 1/2 in · 38 – 89 mm |
| Threads | Not applicable |
| Head / geometry | Flat head, ring or screw shank |
| Materials | Stainless steel 301 / 303 / 304 / 304L / 316 / 316L / 410 / 416 / 17-4PH · carbon steel 1045 / 1215 / 12L14 · alloy steel 4130 / 4140 · aluminium 2024 / 5052 / 6061 / 7075 · brass · bronze · copper · titanium |
| Finishes | As machined · black oxide · zinc plating · nickel plating · chrome plating · anodizing · passivation (through our vetted partner network) |
| Precision | ±0.01 mm on features that locate, seal or fit; ISO 2768-m for general dimensions |
| Marking | Head marking, grade marking or your own identification mark per drawing |
| Documents | Material certificate (MTR) with every batch, plus pre-shipment photos before dispatch |
| MOQ | From 50 pieces per type and material · samples from 1 piece |
| Sample lead time | 5–10 days |
| Production lead time | 25–35 days after sample approval |
| Quote | Within 24 hours, with DFM feedback |
Other nails & spikes we manufacture
See all 179 part types →Send us the drawing
We reply within 24 hours with DFM feedback, a process route and a price. Samples from 1 piece, production from 50 pieces, shipped from Qidong City, Jiangsu Province, China.
Request a quote